Harris 5356 Aluminum Welding Rods 1/16" x 36" 3 lb.
|
Regular Price: $31.80
Your Price: $22.75
You Save: $9.05 (28 %)
Item Number: HAR53563033POP
|
GTAW (TIG) - For manual AC welding, argon is generally preferred because the arc has good stability. On heavier sections, the addition of helium may be considered, and arc penetration will increase significantly; however, gas flow rates must be increased when helium is added.
|
Material Thickness
|
Tungsten, Pure or Zirconiated
|
Wire Size
|
Welding Current (Amps)
|
Arc Voltage
|
Gas Cup
|
Argon, cfh
|
| 1/2"
|
1/4"
|
1/4"
|
400 - 450
|
25
|
5/8"
|
35
|
| 3/8"
|
1/4"
|
3/16" - 1/4"
|
330 - 380
|
15
|
5/8"
|
35
|
| 1/4"
|
3/16" - 1/4"
|
3/16"
|
220 - 275
|
15
|
1/2"
|
30
|
| 3/16"
|
5/32" - 3/16"
|
5/32" - 3/16"
|
170 - 225
|
15
|
7/16" - 1/2"
|
25
|
| 1/8"
|
1/8" - 5/32"
|
1/8" - 5/32"
|
125 - 175
|
15
|
7/16"
|
20
|
| 1/16"
|
1/16" - 3/32"
|
1/16" - 3/32"
|
70 - 100
|
15
|
3/8"
|
20
|
|
|
|